High-Temperature Gas Environment

High-Temperature Gas Environment

The ambient testing cell can be replaced with a furnace for high-temperature gas environment testing. The operation temperature depends on the furnace type, but 800°C temperature is the most typical.


The furnace is not gas-tight, but a continuous gas or gas mixture will be led in the furnace to prevent exposure of the high temperature of the specimen to air. The furnace setup is regularly equipped with adjustable flow meters for nitrogen and an operation gas such as CO2. There is also an adjustable flow meter for the cooling water that controls the pull rod temperature. 